We are a leading Manufacturer of er 347 si stainless steel welding wire, er 316 l si stainless steel welding wire, er 904 l stainless steel welding wire, er 309 l si wire, er 308 h stainless steel welding wire and er 312 stainless steel welding wire from Mumbai, India.

ER 347 Si Stainless Steel Welding Wire

REQUEST CALLBACK

ER 347 Si Stainless Steel Welding Wire
Ask for Price

Thanks for Contacting Us.

Product Price :Get Latest Price

Application:

Stabilised CrNiNb-wire/rod for joining and surfacing corrosion resistant steels/cast steels for service temperatures from –110°C up to + 400°C.

Chemical Composition Element by weight (%):

C: 0,06 Si: 0,85 Mn: 1,30 Cr: 19,50 Ni: 9,50 Nb: 12xC

Mechanical Properties (typical) :

Yield Strength (Re) 490 N/mm²
Tensile Strength (Rm) 680 N/mm²
Elongation (A)(Lo=5do) 32%
Impact energy (Av) 80 J
High temp. 400°C
Low temp. -110°C
Yes! I am interested

ER 316 L Si Stainless Steel Welding Wire

REQUEST CALLBACK

ER 316 L Si Stainless Steel Welding Wire
Ask for Price

Thanks for Contacting Us.

Product Price :Get Latest Price

Application:

CrNiMo-wire/rod with low carbon for joining and surfacing corrosion resistant and sub-zero tough austenitic steels for service temperatures from – 196°C up to + 400°C.

Chemical Composition Element by weight (%):

C: 0,02 Si: 0,85 Mn: 1,80 Cr: 18,5 Ni: 12,5 Mo: 2,60 

Mechanical Properties (typical) :

Yield Strength (Re) 430 N/mm²
Tensile Strength (Rm) 650 N/mm²
Elongation (A)(Lo=5do) 34%
Impact energy (Av) 90 J
High temp. 400° C
Low temp. -196° C
Yes! I am interested

ER 904 L Stainless Steel Welding Wire

REQUEST CALLBACK

ER 904 L Stainless Steel Welding Wire
Ask for Price

Thanks for Contacting Us.

Product Price :Get Latest Price

Application :

Stainless steel; resistant to intercrystalline corrosion and wet corrosion up to 350°C. Good corrosion resistance similar to matching steels/cast steel grades, above all in reducing environments. For joining and surfacing work with matching austenitic CrNiMoCu steels/cast steel grades. For joining these steels with unalloyed/low-alloy steels/cast grades.

Chemical Composition Element by weight (%):

C: 0,02 Si: 0,20 Mn: 2,0 Cr : 20,0 Mo:4,5  Ni: 25,0 Cu: 1,5

Mechanical Properties (typical) :

Yield Strength (Re) 380 N/mm²
Tensile Strength (Rm) 560 N/mm²
Elongation (A)(Lo=5do) 35%
Impact energy (Av) 80 J
High temp. 350° C
Low temp. -196° C
Yes! I am interested

ER 309 L Si Wire

REQUEST CALLBACK

ER 309 L Si Wire
Ask for Price

Thanks for Contacting Us.

Product Price :Get Latest Price

Application:

CrNi-wire/rod with low carbon for joining un-and low alloyed steels/cast steels and austenitic steels resistant to intergranular/wet corrosion to 300°C. Suitable for intermediate layers and for joining dissimilar steels.

Chemical Composition Element by weight (%):

C: 0,02 Si: 0,85 Cr : 24,5 Ni: 13,5 Mn: 1,8  

Mechanical Properties (typical):

Yield Strength (Re) 400 N/mm² 
Tensile Strength (Rm) 600 N/mm²
Elongation (A)(Lo=5do) 30%
Impact energy (Av) 65 J
High temp. 300° C
Low temp. -60° C
Yes! I am interested

ER 308 H Stainless Steel Welding Wire

REQUEST CALLBACK

ER 308 H Stainless Steel Welding Wire
Ask for Price

Thanks for Contacting Us.

Product Price :Get Latest Price

Application :

Hight temparature resistant up to 700°C (1292°F). Resistant to scaling up to 800°C (1472°F). For surfacing and joing applications on matchin/similar high temperature resistant steels/cast steel.

Chemical Composition Element by weight (%) :

 C: 0,06 Si: 0,60 Mn: 1,90 Cr: 20,0 Ni: 9,5 Mo: 0,1 

Mechanical Properties:

Yield Strength (Re) 370 N/mm² 
Tensile Strength (Rm) 570 N/mm²
Elongation (A)(Lo=5do) 35 %
Impact energy (Av) 70 J (20°C) 
Yes! I am interested

ER 312 Stainless Steel Welding Wire

REQUEST CALLBACK

ER 312 Stainless Steel Welding Wire
Ask for Price

Thanks for Contacting Us.

Product Price :Get Latest Price

Application :

CrNi-wire/rod for joining and surfacing equivalent and comparable steels/cast steels and manganese steels. Good resistance to cavitation and thermal cracking. Also for joining dissimilar steels and for repairs/surfacing of hot working tools and intermediate layers.

Chemical Composition Element by weight (%) :

C: 0,12 Si: 0,4 Mn: 1,8 Cr: 30,0 Ni: 9,0 

Mechanical Properties (typical) :

Yield Strength (Re) 560 N/mm²
Tensile Strength (Rm) 740 N/mm²
Elongation (A)(Lo=5do) 25%
High temp. 300° C
Low temp. -60° C
Yes! I am interested

ER 410 NiMo Stainless Steel Welding Wire

REQUEST CALLBACK

ER 410 NiMo Stainless Steel Welding Wire
Ask for Price

Thanks for Contacting Us.

Product Price :Get Latest Price

Application :

Welding of high strength martensitic stainless steel with better resistance to corrosion, hydro-cavitaation and good sub-zero toughness. Welding of 13-Cr-4%Ni alloys in cast or forged form of hydraulic turbines, valve bodies, pump bowls. etc.

Chemical Composition Element by weight (%):

C: 0,05 Si: 0,60 Mn: 0,60 Cr: 13,5 Ni: 4,5 Mo: 0,50 

Mechanical Properties (typical) :

 Yield Strength (Re) 600 N/mm²
Tensile Strength (Rm) 800 N/mm²
Elongation (A)(Lo=5do) 15 %
Impact energy (Av) 50 J
Hardness 250 HB 
Yes! I am interested

ER 309 L Mo Stainless Steel Welding Wire

REQUEST CALLBACK

ER 309 L Mo Stainless Steel Welding Wire
Ask for Price

Thanks for Contacting Us.

Product Price :Get Latest Price

Application

CrNi-wire/rod with low carbon for joining un-and low alloyed steels/cast steels and austenitic steels resistant Suitable for intermediate layers and for joining dissimilar steels.

Chemical Composition Element by weight (%) :

C :0,02 Si :0,35 Cr :22 Ni :14 Mn :1,5 Mo :2,6 

Mechanical Properties (typical) :

Yield Strength (Re) 480 N/mm²
Tensile Strength (Rm) 600 N/mm²
Elongation (A)(Lo=5do) 30 %
Impact energy (Av) 65 J
Hardness 210 HB
High temp. 300° C
Low temp. -10° C
Yes! I am interested

ER 317L Stainless Steel Welding Wire

REQUEST CALLBACK

ER 317L Stainless Steel Welding Wire
Ask for Price

Thanks for Contacting Us.

Product Price :Get Latest Price

Application : 

Welding of 317/317L stainless steels in which the Raised Mo level provides improved resistance to pitting in high chloride environments and to some acids (no nitric acid).

Chemical Composition Element by weight (%):

C: 0,03 Si: 0,4 Mn:1,4 Cr: 19 Ni:14 Mo: 3,5 

Mechanical Properties (typical) : 

0,1%-proof stress 370 N/mm²
0,2%-proof stress 350 N/mm²
Tensile Strength 570 N/mm²
Elongation (A)(Lo=5do) 34%
Impact energy (+20°C) 55J 
Yes! I am interested

 
X


Explore More Products

Contact via E-mail
Contact via SMS
Sahara Enterprises
Bhavesh Shah (Director Marketing)
G/17, 1st Floor, Sarvodaya Nagar Building 1st Panjarapole Lane, C.P. Tank, Bhuleshwar,
Mumbai - 400004, Maharashtra, India
Call Us: 
Call Response Rate: 85%
Share Us :
F G T L



Home  |   About Us   |  Our Products  |  Site Map  |   Contact Us

© Sahara Enterprises. All Rights Reserved (Terms of Use)
Developed and Managed by IndiaMART InterMESH Limited

Sahara Enterprises